Abstract

To compare the transverse strength and impact strength of a high impact heat cure denture base resin with that of a conventional heat cure denture base resin reinforced with E-glass and polyethylene fibers. To investigate the relative efficacy of addition of E-glass and polyethylene fibers in improving the impact and transverse strength of a commercially available conventional heat cure resin and compare that with high impact heat cure denture base resin. 80 het cure denture base resin blocks samples; 20 of conventional heat cure denture base resin (DPI India), 20 of high impact heat cure denture base resin (Trevalon High Impact, Dentsply International, Germany), 20 of E-glass fiber(India chemicals limited, Ahmadabad, India) reinforced heat cure denture base resin and 20 of polyethylene (India chemicals limited, Ahmadabad, India)  reinforced heat cure denture base resin respectively) were tested with Lloyd’s instrument material (Milano, Italy Model No. LR 100K) for transverse strength and Charpy digital impact tester (Milano, Italy Model No. IZOD 44) for impact strength. There was significant increase in transverse and impact strength values of conventional heat cure denture base resin reinforced with E-glass and polyethylene fibers. However transverse strength of high impact heat cure denture base resin was still higher than conventional heat cure denture base resin reinforced with E-glass and polyethylene fibers.

References

Anusavice K J. Philips science of Dental Materials, XI edition

Rahamneh A, Jagger D.C. Effect on addition of different fibers on transverse strength and impact strength of acrylic resin base material. Euro Pros Rest Dent. 2003

Mona K M. Reinforcement of denture base resin with glass fillers. J Prosthet Dent 1981;46:232-240

Sir Ha Foo et al. Effect of fiber reinforcement on the strength of three denture base resins. JOP 2005;10:148-53

Stipho HD. Repair of acrylic resin denture base reinforced with glass fiber. J Prosthet Dent 1998;79(5):580-84

Beyli MS, Franhofer JA. An analysis of cause of fracture of acrylic resin denture. J Prosthet Dent 1981;46:236-40

Craig RG, Powers JM. Restorative dental materials. XI edition

Ferracane JL. Materials in dentistry. Principles and application. II edition.

Published

2015-02-28

How to Cite

Iqbal, U. ., & Amin Naqash, T. . (2015). Comparison of transverse strength and impact strength of a high impact heat cure denture base resin with that of a conventional heat cure denture base resin reinforced with e-glass and polyethylene fibers. Scientific Journal of Review, 4(2), 17-21. Retrieved from http://sjournals.com/index.php/sjr/article/view/444

Issue

Section

Engineering